Abstract :
The rare-earth sulfide NdGdS3 with Th3P4-type structure was prepared by heating a mixture of Nd2O3 and Gd2O3 in a stream of CS3/Ar at 1273 K, followed by sintering at 1873 K. In order to evaluate the potential for thermoelectric applications, the electrical resistivity and the Seebeck coefficient were measured over the temperature range of 300 to 1000 K. The Seebeck coefficient is negative over the whole temperature range measured. The electrical resistivity and the magnitude of Seebeck coefficient increase linearly with increasing temperature. The thermoelectric power factor also increases with increasing temperature to a maximum value of 180 muW/K2middotm at 923 K
Keywords :
Seebeck effect; electrical resistivity; gadolinium alloys; neodymium alloys; sintering; thermoelectric power; 1273 K; 1873 K; 300 to 1000 K; NdGdS3; Seebeck coefficient; electrical resistivity; rare-earth sulfide; sintering; thermoelectric power factor; thermoelectric property; Argon; Atmosphere; Electric resistance; Heating; Lattices; Materials science and technology; Powders; Solids; Temperature; Thermoelectricity;
fLanguage :
English
Publisher :
ieee
Conference_Titel :
Thermoelectrics, 2006. ICT '06. 25th International Conference on
Conference_Location :
Vienna
ISSN :
1094-2734
Print_ISBN :
1-4244-0811-3
Electronic_ISBN :
1094-2734
Type :
conf
DOI :
10.1109/ICT.2006.331378
Filename :
4133357
Link To Document :
بازگشت