Abstract :
We report Seebeck coefficient, S(T) and electrical resistivity, ρ(T) measurements of Bi0.88Sb0.12 compounds prepared by mechanical alloying (MA). The behavior of the Seebeck coefficient and electrical resistivity were studied as a function of temperature and the milling time (MT). The milling process was carried out at room temperature and took different values from 0 hours to 45 hours. The Seebeck coefficient was measured by using the differential method in the temperature range between 77 K and 300 K. S(T) is negative in whole temperature range measured and it changes from -60 μV/K for the samples with low milling time up to reach values close to -160 μV/K in the samples processed through 45 hours. The thermoelectric power factor, PF increases with the temperature and the milling time, it reaches values close to 5 μW/K2cm. This result allows us to consider the use of this simple and inexpensive method to grow this kind of thermoelectric materials.
Keywords :
Seebeck effect; antimony alloys; bismuth alloys; electrical resistivity; mechanical alloying; milling; semiconductor materials; thermoelectric power; 0 to 45 hour; 77 to 300 K; Bi0.88Sb0.12; Seebeck coefficient; differential method; electrical resistivity; mechanical alloying; milling; thermoelectric power; Alloying; Bismuth; Electric resistance; Electric variables measurement; Mechanical variables measurement; Milling; Temperature distribution; Temperature measurement; Thermoelectricity; Time measurement;
fLanguage :
English
Publisher :
ieee
Conference_Titel :
Thermoelectrics, 2005. ICT 2005. 24th International Conference on
ISSN :
1094-2734
Print_ISBN :
0-7803-9552-2
Type :
conf
DOI :
10.1109/ICT.2005.1519970
Filename :
1519970
Link To Document :
بازگشت