Changes of space charge profiles in PET electrets after thermally stimulated discharges
Author
Moty, E.
Author_Institution
Inst. of Electr. Eng. Fundamentals, Wroclaw Univ. of Technol., Poland
fYear
2002
fDate
2002
Firstpage
247
Lastpage
250
Abstract
Behaviour of electric charges in a PET film has been investigated under the condition of partial discharging at higher annealing temperatures. The PET electrets corona-charged at room temperature and 440 K were investigated. The step electroacoustic method was used for the measurement of the space charge distributions along the sample thickness. The highest surface charge densities, and charge stability were obtained after negative corona charging at 440 K.
Keywords
charge measurement; corona; electrets; partial discharges; polymer films; space charge; thermally stimulated currents; 440 K; PET electrets; PET film; annealing temperatures; charge stability; corona-charged electrets; electric charges; negative corona charging; partial discharging; space charge distribution measurement; space charge profiles; step electroacoustic method; Annealing; Charge measurement; Current measurement; Electrets; Positron emission tomography; Space charge; Surface charging; Surface discharges; Temperature; Thickness measurement;
fLanguage
English
Publisher
ieee
Conference_Titel
Electrets, 2002. ISE 11. Proceedings. 11th International Symposium on
Print_ISBN
0-7803-7560-2
Type
conf
DOI
10.1109/ISE.2002.1042989
Filename
1042989
Link To Document