Abstract :
40μm silver-silver indium (Ag-AgIn) flip-chip interconnect process at 180°C by transient liquid phase (TLP) bonding process is reported. Array of 50×50 flip-chip joints with 100μm pitch and 40μm joint diameter was fabricated on silicon (Si) and bonded to copper (Cu) substrate at 180°C for 5 minutes with a static pressure of 0.4-0.7MPa (60-100psi). The corresponding load for each joint is 0.05gm. In the bonding, no flux was used. Cross section SEM images show that Ag columns are well bonded to the Cu substrate without visible voids or cracks. EDX data indicate that the resulting column structure is Ag/(Ag)/Ag2In/(Ag). Each joint has height approximately 50μm. In this structure, Ag2In is a dominating intermetallic compound (IMC) in the Ag-In system with melting temperature of 660°C. (Ag) is a solid solution phase of Ag with In composition up to 20 at. %. It has a solidus temperature range of 695 to 962°C depending on In composition. In long-term operation, (Ag)/Ag2In/(Ag) is expected to gradually convert to a single (Ag) phase which is more reliable. Thus, the flip-chip joints will get better in use. The process temperature of this new interconnect method is 80°C below typical reflow temperature of tin-based lead-free solders. The free shear strain of this 50μm Ag-AgIn flipchip interconnect between Si and Cu is around 0.14. This strain value is relatively small for ductile material such as Ag.
Keywords :
X-ray chemical analysis; bonding processes; copper; flip-chip devices; indium alloys; integrated circuit interconnections; reflow soldering; scanning electron microscopy; silicon; silver; silver alloys; Ag-AgIn; Cu; EDX; Si; energy dispersive X-ray analysis; flip chip joints; flip-chip interconnect process; free shear strain; intermetallic compound; lead-free solders; melting temperature; pressure 0.4 MPa to 0.7 MPa; process temperature; reflow temperature; scanning electron microscopy; size 100 mum; size 40 mum; temperature 180 degC; temperature 660 degC; temperature 695 degC to 962 degC; time 5 min; transient liquid phase bonding process; Bonding; Flip chip; Indium; Joints; Silicon; Solids; Substrates; electronic packaging; flip-chip; flip-chip interconnect; flip-chip technology; fluxless bonding; indium; silver;
fLanguage :
English
Publisher :
ieee
Conference_Titel :
Electronic Components and Technology Conference (ECTC), 2012 IEEE 62nd
Conference_Location :
San Diego, CA
ISSN :
0569-5503
Print_ISBN :
978-1-4673-1966-9
Electronic_ISBN :
0569-5503
Type :
conf
DOI :
10.1109/ECTC.2012.6248892
Filename :
6248892
Link To Document :
بازگشت