• DocumentCode
    2829518
  • Title

    Conversion of a 3000 TPD planetary cooler kiln to grate cooler in less than 50 days

  • Author

    Lund, By Ray

  • Author_Institution
    Irish Cement Ltd., Ireland
  • fYear
    1999
  • fDate
    1999
  • Firstpage
    269
  • Lastpage
    278
  • Abstract
    In October 1995 a total of seven serious cracks were discovered on the tyre uphill of the planetary coolers (Tyre 2) and two smaller cracks on the tyre downhill of the coolers (Tyre 1) of the Platin cement plant of Irish Cement Limited (ICL). New tyres were ordered immediately, and an evaluation of the possible causes was undertaken. No mathematical reason for the cracks could be discovered, the story throughout the industry being that such cracks could be expected at the age and duty history of the kiln. This paper describes the option of replacing the entire planetary cooler arrangement with a grate cooler which was examined as a potential alternative to the repair of the above
  • Keywords
    cement industry; cooling; industrial power systems; maintenance engineering; project engineering; Ireland; cement plant; conversion project; grate cooler; maintenance; planetary cooler kiln; replacement; Building materials; Cement industry; Fatigue; History; Kilns; Principal component analysis; Surgery; Tires; USA Councils; Welding;
  • fLanguage
    English
  • Publisher
    ieee
  • Conference_Titel
    Cement Industry Technical Conference, 1999. Conference Record. 1999 IEEE-IAS/PCA
  • Conference_Location
    Roanoke, VA
  • ISSN
    1079-9931
  • Print_ISBN
    0-7803-5523-7
  • Type

    conf

  • DOI
    10.1109/CITCON.1999.767042
  • Filename
    767042