• DocumentCode
    3288796
  • Title

    Development of silica aerogel with any density

  • Author

    Tabata, M. ; Adachi, I. ; Fukushima, T. ; Kawai, H. ; Kishimoto, H. ; Kuratani, A. ; Nakayama, H. ; Nishida, S. ; Noguchi, T. ; Okudaira, K. ; Tajima, Y. ; Yano, H. ; Yokogawa, H. ; Yoshida, H.

  • Author_Institution
    Graduate Sch. of Sci. & Technol., Chiba Univ.
  • Volume
    2
  • fYear
    2005
  • fDate
    23-29 Oct. 2005
  • Firstpage
    816
  • Lastpage
    818
  • Abstract
    New production methods of silica aerogel with high and low refractive indices have been developed. A very slow shrinkage of alcogel at room temperature has made possible producing aerogel with high refractive indices of up to 1.265 without cracks. Even higher refractive indices than 1.08, the transmission length of the aerogel obtained from this technique has been measured to be about 10 to 20 mm at 400 nm wave length. A mold made of alcogel which endures shrinkage in the supercritical drying process has provided aerogel with the extremely low density of 0.009 g/cm3, which corresponds to the refractive index of 1.002. We have succeeded producing aerogel with a wide range of densities
  • Keywords
    aerogels; drying; refractive index; silicon compounds; 10 to 20 mm; SiO2; alcogel; refractive indices; silica aerogel; supercritical drying process; transmission length; Annealing; Glass; Instruction sets; Length measurement; Production; Protons; Refractive index; Silicon compounds; Solvents; Temperature;
  • fLanguage
    English
  • Publisher
    ieee
  • Conference_Titel
    Nuclear Science Symposium Conference Record, 2005 IEEE
  • Conference_Location
    Fajardo
  • ISSN
    1095-7863
  • Print_ISBN
    0-7803-9221-3
  • Type

    conf

  • DOI
    10.1109/NSSMIC.2005.1596380
  • Filename
    1596380