Coarsening of Bi phase and intermetallic layer thickness in Sn-58Bi-X (X=In and Ni) solder joint
Author :
Mokhtari, O. ; Nishikawa, Hisashi
Author_Institution :
Joining & Welding Res. Inst., Osaka Univ., Ibaraki, Japan
fYear :
2013
fDate :
11-14 Aug. 2013
Firstpage :
250
Lastpage :
253
Abstract :
The use of Pb has been limited in the electronic industry because of the toxicity of lead. Sn-Bi-based alloys are alternatives to replace Pb-based solders in the low temperature ranges. However, Sn-Bi-based solders show brittle behavior in both the bulk and the interface. Generally, the addition of impurity elements to the solders can improve the ductility of the solder joint in both the bulk and the interface by refining the solder microstructure and suppressing the intermetallics at the interface, respectively. In this study, the effect of third elements, i.e., Ni and In (1 and 0.5wt.%) on the microstructure of the Sn-58Bi solder and thickness of the intermetallic compound (IMC) at the interface between Sn-58Bi solder and Cu substrate after the reflow and 1, 3 and 6 weeks of aging at 80 °C were investigated. The joint strength of the new solder alloys were also investigated.
Keywords :
bismuth alloys; indium alloys; lead alloys; nickel alloys; reflow soldering; solders; tin alloys; IMC; In; Ni; Pb; Sn-Bi; electronic industry; impurity elements; intermetallic compound; intermetallic layer; reflow; solder alloys; solder joint; solder microstructure; temperature 80 C; time 1 week; time 3 week; time 6 week; Aging; Bismuth; Intermetallic; Microstructure; Nickel; Soldering; Bi coarsening; Sn-Bi solder; ductility; intermetallic layer;
fLanguage :
English
Publisher :
ieee
Conference_Titel :
Electronic Packaging Technology (ICEPT), 2013 14th International Conference on
Conference_Location :
Dalian
Type :
conf
DOI :
10.1109/ICEPT.2013.6756465
Filename :
6756465
Link To Document :
بازگشت