• DocumentCode
    3535207
  • Title

    Erosion of ATH and silica filled silicone rubber in the DC inclined plane test

  • Author

    Ghunem, R.A. ; Jayaram, S.H. ; Cherney, E.A.

  • Author_Institution
    Electr. & Comput. Eng. Dept., Univ. of Waterloo, Waterloo, ON, Canada
  • fYear
    2012
  • fDate
    24-28 July 2012
  • Firstpage
    1
  • Lastpage
    4
  • Abstract
    In this paper erosion of silicone rubber loaded with 30 wt% ATH and silica is investigated in the DC inclined plane tracking/erosion test as per ASTM D 2303. Reduced equivalent DC voltages have been applied in order to compare with the erosion under AC. Hot spot temperatures are used for comparative analysis of dry-band arcing severity on the tested materials. Also, depending on the type of filler, initiation of stable and intense dry-band arcing is discussed. Based on the results it is proposed that the existing material formulation used for AC insulators are not suitable for DC insulators as the erosion is more severe and different.
  • Keywords
    arcs (electric); silicone rubber insulators; ASTM D 2303; ATH erosion; DC inclined plane test; DC insulators; comparative analysis; dry-band arcing severity; hot spot temperature; silica filled silicone rubber; Degradation; Insulation life; Materials; Materials reliability; Silicon compounds; Thermal conductivity; ASTM D2303; ATH; DC inclined plane test; Dry-band arcing; Erosion; Hot spot; Silica;
  • fLanguage
    English
  • Publisher
    ieee
  • Conference_Titel
    Properties and Applications of Dielectric Materials (ICPADM), 2012 IEEE 10th International Conference on the
  • Conference_Location
    Bangalore
  • ISSN
    2160-9225
  • Print_ISBN
    978-1-4673-2852-4
  • Type

    conf

  • DOI
    10.1109/ICPADM.2012.6318916
  • Filename
    6318916