• DocumentCode
    633482
  • Title

    Optical amplification at 1.3 µm with Bi doped fiber fabricated by VAD method

  • Author

    Takahashi, Masaharu ; Fujii, Teruya ; Saito, Yuya ; Fujii, Yuka ; Kobayashi, S.

  • Author_Institution
    Chitose Inst. of Sci. & Technol., Chitose, Japan
  • fYear
    2013
  • fDate
    June 30 2013-July 4 2013
  • Firstpage
    1
  • Lastpage
    2
  • Abstract
    In this report an optical amplification with Bi doped silica fiber (BDF) fabricated by the Vapor Axial Deposition (VAD) method is presented. Bi concentration is measured as 0.07-1 mol%. The measured amplified gain was 6 dB with input low laser power at 1.3 μm using a double cladding BDF of 2 m.
  • Keywords
    bismuth; optical fibre amplifiers; optical fibre cladding; optical fibre fabrication; silicon compounds; vapour deposition; Bi concentration; Bi doped silica fiber; SiO2:Bi; VAD method; double cladding BDF; gain 6 dB; optical amplification; vapor axial deposition; wavelength 1.3 mum; Photonics; Switches;
  • fLanguage
    English
  • Publisher
    ieee
  • Conference_Titel
    OptoElectronics and Communications Conference held jointly with 2013 International Conference on Photonics in Switching (OECC/PS), 2013 18th
  • Conference_Location
    Kyoto
  • Type

    conf

  • Filename
    6597617