    Experimental Demagnetizing Factors for Disk Samples Magnetized Along a Diameter

  • Author

    Graham, C.D. ; Lorenz, Bryen E.

  • Author_Institution
    Dept. of Mater. Sci. & Eng., Pennsylvania Univ., Philadelphia, PA
  • Volume
    43
  • Issue
    6
  • fYear
    2007
  • fDate
    6/1/2007 12:00:00 AM
  • Firstpage
    2743
  • Lastpage
    2745
  • Abstract
    Demagnetizing factors for disk samples of a commercial 80Ni permalloy have been measured using a vibrating sample magnetometer with fields provided by a Helmholtz coil pair. The range of values of m (diameter/thickness) is from 12.5 to 385. The experimental values of N are significantly higher than those calculated for an ellipsoid, but lower than those calculated assuming uniform magnetization
  • Keywords
    Permalloy; demagnetisation; ferromagnetic materials; Helmholtz coil pair; NiFe; commercial 80Ni Permalloy; demagnetizing factors; disk samples; magnetization; vibrating sample magnetometer; Coils; Demagnetization; Ellipsoids; Magnetic field measurement; Magnetic flux; Magnetic materials; Magnetometers; Saturation magnetization; Superconducting magnets; Vibration measurement; Demagnetizing factors; magnetic measurements; vibrating sample magnetometer;
  • fLanguage
    English
  • Journal_Title
    Magnetics, IEEE Transactions on
  • Publisher
    ieee
  • ISSN
    0018-9464
  • Type

    jour

  • DOI
    10.1109/TMAG.2007.893854
  • Filename
    4202740