Samarium-cobalt magnets resistant to 750°C
Author :
Kumar, K. ; Das, D. ; Wettstein, E.
Author_Institution :
IEEE TMAG
Volume :
14
Issue :
5
fYear :
1978
fDate :
9/1/1978 12:00:00 AM
Firstpage :
788
Lastpage :
790
Abstract :
Hcilosses in high coercivity plasma-sprayed samarium-cobalt magnets (at temperatures of 700 to 800°C) are much less severe than those observed for sintered magnets. Magnets with initial coercivities of about 60 kOe show values of 35 to 50 kOe, after exposures of several hundred hours to temperatures of 700 and 750°C. The data collected on sprayed magnets indicates that Hcilosses at these temperatures can be related to a narrowing SmCo5homogeneity range and to processes involving oxygen dissolution and precipitation. These losses do not result from eutectoid decomposition of the SmCo5phase as is widely accepted. The findings of this study will find extensive use in the development of thermal processing techniques that will employ slow cooling of magnets from elevated temperatures.
Keywords :
Coercive forces; Magnetic thermal factors; Permanent magnet motors; Aging; Cobalt; Coercive force; Heat treatment; Human computer interaction; Magnets; Plasma properties; Plasma temperature; Spraying; Temperature distribution;
fLanguage :
English
Journal_Title :
Magnetics, IEEE Transactions on
Publisher :
ieee
ISSN :
0018-9464
Type :
jour
DOI :
10.1109/TMAG.1978.1060002
Filename :
1060002
Link To Document :
بازگشت