عنوان مقاله :
مقايسه خواص جرم هاي ريختني آلومينا - اسپينل با آلومينا - منيزيا
عنوان به زبان ديگر :
Comparision of Alumina-Spines and Alumina-Magnesia Castable Refractory properties
پديد آورندگان :
نقي زاده ، رحيم مترجم ,
اطلاعات موجودي :
فصلنامه سال 1384 شماره 21
كليدواژه :
Comparision , Alumina-Magnesia , جرم هاي آلومينا - اسپينل , Alumina-Spines , مهندسي , Castable , جرم هاي آلومينا - منيزيا , deflocculation
چكيده لاتين :
Nowadays, Industrial application of alumina-magnesia and alumina-spinel castable refractories in secondary ladle metallurgy is under expanding. Itʹs mentioned that alumina-magnesia castable has better corrosion resistance and alumina-spinet castable has good thermal shock properties. The goal of this study was the determination of spinet formation control enhancing the thermal shock properties of alumina-magnesia castable refractories.ln this study alumina - magnesia castable whit 5-7% dead-bum magnesia were compared with alumina-spinel castabe with 10-17% spinet from point of view of cold modulus of rupture, thermal shock properties; phase and microstructural analysis. The particle size distribution In both castables were on the base on Anderiasen equation whit q=0.3. The cement content in each castable was 5% wt and the used deflocculant was sodium hexa meta phosphate. The results showed that the deflocculation of alumina- magnesia castable was difficult and the loss of some properties could be related to it. With thermal shock about 1250°C, the loss of strength in alumina magnesia containing samples up to 5 cycles could be seen and that was more than alumina-spine] containing samples. But after 10 thermal shock cycles, the strength variations were the same.
عنوان نشريه :
مهندسي متالورژي
عنوان نشريه :
مهندسي متالورژي
اطلاعات موجودي :
فصلنامه با شماره پیاپی 21 سال 1384
كلمات كليدي :
#تست#آزمون###امتحان